Process for the recovery of nickel and/or cobalt from high ferrous content laterite ores
A Provisional patent application filed on 20 March 2008 credited to Not Given
Details
Application number :
2008901412
Application type :
Provisional
Application status :
LAPSED
Under opposition :
No
Proceeding type :
Invention title :
Process for the recovery of nickel and/or cobalt from high ferrous content laterite ores